BSI BS HR 506:1989

Nickel-chromium-cobalt-titanium-aluminium heat-resisting alloy wire: softened (nickel base, Cr 19.5, Co 18, Ti 2.5, Al 1.5)

PUBLISH DATE 1989
PAGES 4
BSI BS HR 506:1989
REAFFIRMED 2009
Chemical composition, mechanical properties, inspection and test requirement for a softened wire for use as locking wire.