ISO 806:2004

Current Revision
Aluminium oxide primarily used for the production of aluminium - Determination of loss of mass at 300 degrees C and 1 000 degrees C

Best Price Guarantee Oct 15, 2004 English 1 Pages

Sub Total (1 Item(s)) $ 0.00
Estimated Shipping $ 0.00
Total (Pre-Tax) $ 0.00

You own the digital copy of this edition

View in Library
or
International Organization for Standardization Logo

ISO 806:2004

Aluminium oxide primarily used for the production of aluminium - Determination of loss of mass at 300 degrees C and 1 000 degrees C

PUBLISH DATE 2004
ISO 806:2004

ISO 806:2004 specifies a method for the determination of loss of mass on heating of aluminium oxide at 300 °C and further loss of mass on ignition at 1 000 °C. By industry convention, these mass losses are often referred to as "moisture (MOI)" and "loss on ignition (LOI)" respectively.

This method is suitable for calcined alumina in the range 0,2 % to 5 % loss of mass at 300 °C and 0,1 % to 2 % loss of mass at 1 000 °C.

This method provides for samples to be treated on an "as-received" basis for determination of actual MOI and LOI in alumina samples. To improve precision of analysis in cases where "as-received" results are not required, samples can be "air-equilibrated" prior to analysis. "Air-equilibration" can greatly affect MOI results and significantly alter LOI results. The "air-equilibration" procedure and its effects are discussed.

Instrumental methods are also discussed.