Ductile (Nodular) Iron Castings, Sand 80,000 psi (550 MPa) Tensile Strength As Cast
Steel Castings, Investment 0.80Cr - 1.8Ni - 0.35Mo (0.28 - 0.36C) (SAE 4330 Modified) Annealed
Steel Castings, Sand, 0.80cr 1.8ni 0.35mo (0.28-0.36c) Annealed
Steel, Sand, Castings, 0.82cr 1.8ni 0.35mo (0.38-0.46c) Normalized and Tempered
Steel, Investment Castings 0.50Cr - 0.55Ni - 0.25Mo (0.11 - 0.17C) (SAE 8615) Normalized
Steel Castings, Sand, 0.65Cr - 0.75Ni - 0.20Mo (0.25 - 0.33C) (SAE 8630 Modified) Normalized and Tempered
Steel, Maraging, Investment Castings 18.5Ni - 9.0Co - 5.0Mo - 0.70Ti - 0.12Al Vacuum Melted Homogenized, Overaged, and Solution Heat Treated
Steel Castings, Investment, Corrosion Resistant 19.5Cr - 10.5Ni - 0.25S (Type 303) Solution Heat Treated
Centrifugal Steel Castings Chromium Molybdenum 38-45
Steel Castings, Tubular, Centrifugal, Corrosion Resistant 15Cr - 4.6Ni - 0.22 (Cb+Ta) - 2.8Cu Solution Heat Treated
Steel, Corrosion-Resistant, Investment Castings, 13Cr (Alloy 60416), Free Machining; Hardened and Tempered
Steel Castings, Sand, Corrosion and Moderate Heat Resistant 13Cr Normalized and Tempered
Steel, Corrosion-Resistant, Investment Castings, 17Cr - 0.55Mo (0.95 - 1.20C) (440C), Annealed
Steel, Corrosion-Resistant, Investment Castings, 16Cr - 1.9Ni - 0.08N (431), As Cast
Steel Castings, Investment, Corrosion Resistant 18Cr - 9Ni Solution Heat Treated
Steel Castings, Sand, Corrosion and Heat Resistant, 15cr 4.0ni 2.3mo 0.08n, Solution Heat Treated
Steel Castings, Sand and Centrifugal, Corrosion and Heat Resistant, 18.5Cr - 13.5Ni - 2.1Mo, Solution Heat Treated
Steel Castings, Sand and Centrifugal, Corrosion and Heat Resistant 18.5Cr - 10.5Ni - 0.90 (Cb+Ta) Solution Heat Treated
Steel Castings, Sand, Corrosion and Heat Resistant 19.5Cr - 9.5Ni - 1.4Mo - 1.4W - 0.50 (Cb+Ta) - 0.32Ti Solution and Precipitation Heat Treated
Steel Castings, Sand, Corrosion and Heat Resistant, 19.5Cr - 9.5Ni (Low Carbon) (304L) Solution Heat Treated
Steel Castings, Sand, Corrosion Resistant 16Cr - 1.9Ni (Type 431 Mod) Normalized and Tempered
Alloy Castings, Sand, Corrosion and Heat Resistant 16Co - 29Cr - 4.5W As Cast
Alloy Castings, Investment, Corrosion and Heat Resistant 65.5Co - 25Cr - 1.8Ni - 5.0W As Cast
Alloy, Corrosion- and Heat-Resistant, Investment Castings 30Fe - 21Cr - 20Ni - 20Co - 3.0Mo - 2.5W - 1.0Cb - 0.15N (N-155) As-Cast
Nickel Alloy, Corrosion- and Heat-Resistant, Investment Castings 73Ni - 12Cr - 4.5Mo - 2.0Cb (Nb) - 0.70Ti - 0.05C - 6.0Al - 0.010 - 0.10Zr (IN-713 - Low Carbon) Vacuum Cast, As-Cast