SAE AMS5841 Rev G

Current Revision
Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated for Work Strengthening

Best Price Guarantee Feb 3, 2022 English 6 Pages

Sub Total (1 Item(s)) $ 0.00
Estimated Shipping $ 0.00
Total (Pre-Tax) $ 0.00

You own the digital copy of this edition

View in Library
or
SAE International Logo

SAE AMS5841 Rev G

Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated for Work Strengthening

PUBLISH DATE 2022
PAGES 6
SAE AMS5841 Rev G

This specification covers a high strength, corrosion and heat-resistant cobalt-nickel-chromium alloy in the form of bars (see 8.4).